<?xml version='1.0' encoding='utf-8'?>
<documents xmlns='http://eprints.org/ep2/data/2.0'>
  <document id='https://researchdata.bath.ac.uk/id/document/16086'>
    <docid>16086</docid>
    <rev_number>2</rev_number>
    <files>
      <file id='https://researchdata.bath.ac.uk/id/file/53448'>
        <fileid>53448</fileid>
        <datasetid>document</datasetid>
        <objectid>16086</objectid>
        <filename>FigS6_Dofr_ND_50molpc_SiO2_part4.agr</filename>
        <mime_type>text/plain</mime_type>
        <hash>e0c06b1dfca3a351f25740b85b4ef709</hash>
        <hash_type>MD5</hash_type>
        <filesize>649941</filesize>
        <mtime>2022-05-30 16:51:40</mtime>
        <url>https://researchdata.bath.ac.uk/1139/59/FigS6_Dofr_ND_50molpc_SiO2_part4.agr</url>
      </file>
    </files>
    <eprintid>1139</eprintid>
    <pos>59</pos>
    <placement>59</placement>
    <mime_type>text/plain</mime_type>
    <format>other</format>
    <formatdesc>Figure S6 shows the fitted neutron D&apos;(r) functions for several of the MgAS glasses with 50 mol% silica.</formatdesc>
    <language>en</language>
    <security>public</security>
    <license>cc_by</license>
    <main>FigS6_Dofr_ND_50molpc_SiO2_part4.agr</main>
    <content>data</content>
  </document>
</documents>