<?xml version='1.0' encoding='utf-8'?>
<documents xmlns='http://eprints.org/ep2/data/2.0'>
  <document id='https://researchdata.bath.ac.uk/id/document/16309'>
    <docid>16309</docid>
    <rev_number>2</rev_number>
    <files>
      <file id='https://researchdata.bath.ac.uk/id/file/54744'>
        <fileid>54744</fileid>
        <datasetid>document</datasetid>
        <objectid>16309</objectid>
        <filename>Fig1_XRD_Sofk_v3.agr</filename>
        <mime_type>text/plain</mime_type>
        <hash>fa29f0bc7b8d6dad64b322f1e7310be7</hash>
        <hash_type>MD5</hash_type>
        <filesize>341023</filesize>
        <mtime>2022-08-29 15:44:40</mtime>
        <url>https://researchdata.bath.ac.uk/1192/1/Fig1_XRD_Sofk_v3.agr</url>
      </file>
    </files>
    <eprintid>1192</eprintid>
    <pos>1</pos>
    <placement>1</placement>
    <mime_type>text/plain</mime_type>
    <format>other</format>
    <formatdesc>Figure 1 shows the The S_X(k) functions measured for diopside glass and for several of the MgAS glasses containing either ^{nat}Mg or ^{25}Mg.</formatdesc>