<?xml version='1.0' encoding='utf-8'?>
<documents xmlns='http://eprints.org/ep2/data/2.0'>
  <document id='https://researchdata.bath.ac.uk/id/document/17049'>
    <docid>17049</docid>
    <rev_number>2</rev_number>
    <files>
      <file id='https://researchdata.bath.ac.uk/id/file/59905'>
        <fileid>59905</fileid>
        <datasetid>document</datasetid>
        <objectid>17049</objectid>
        <filename>Fig11_Dofr_XRD_50molpc_SiO2_part1_v3.agr</filename>
        <mime_type>text/plain</mime_type>
        <hash>3abe0f88775dca6c072f411e8b157cf0</hash>
        <hash_type>MD5</hash_type>
        <filesize>1587418</filesize>
        <mtime>2023-04-07 15:51:27</mtime>
        <url>https://researchdata.bath.ac.uk/1200/52/Fig11_Dofr_XRD_50molpc_SiO2_part1_v3.agr</url>
      </file>
    </files>
    <eprintid>1200</eprintid>
    <pos>52</pos>
    <placement>52</placement>
    <mime_type>text/plain</mime_type>
    <format>other</format>
    <formatdesc>Figure 11 shows the fitted D&apos;_X(r) functions for the lower alumina content ZnAS glasses with 50 mol% silica.</formatdesc>
    <language>en</language>
    <security>public</security>
    <license>cc_by</license>
    <main>Fig11_Dofr_XRD_50molpc_SiO2_part1_v3.agr</main>
    <content>data</content>
  </document>
</documents>