<?xml version='1.0' encoding='utf-8'?>
<documents xmlns='http://eprints.org/ep2/data/2.0'>
  <document id='https://researchdata.bath.ac.uk/id/document/17710'>
    <docid>17710</docid>
    <rev_number>2</rev_number>
    <files>
      <file id='https://researchdata.bath.ac.uk/id/file/65238'>
        <fileid>65238</fileid>
        <datasetid>document</datasetid>
        <objectid>17710</objectid>
        <filename>Fig9_Dofr_FOD.agr</filename>
        <mime_type>text/plain</mime_type>
        <hash>74801c76675500ac8f9fa4b19a776177</hash>
        <hash_type>MD5</hash_type>
        <filesize>347321</filesize>
        <mtime>2024-01-02 15:23:34</mtime>
        <url>https://researchdata.bath.ac.uk/1238/50/Fig9_Dofr_FOD.agr</url>
      </file>
    </files>
    <eprintid>1238</eprintid>
    <pos>50</pos>
    <placement>50</placement>
    <mime_type>text/plain</mime_type>
    <format>other</format>
    <formatdesc>Figure 9 shows the fitted Delta D&apos;_{Mg}(r) functions for glassy MgAS_37.5_50 at ambient pressure, 3.9 GPa, 8.2 GPa or recovered to ambient conditions from 8.2 GPa.</formatdesc>
    <language>en</language>
    <security>public</security>
    <license>cc_by</license>
    <main>Fig9_Dofr_FOD.agr</main>
    <content>data</content>
  </document>
</documents>