<?xml version='1.0' encoding='utf-8'?>
<documents xmlns='http://eprints.org/ep2/data/2.0'>
  <document id='https://researchdata.bath.ac.uk/id/document/8749'>
    <docid>8749</docid>
    <rev_number>3</rev_number>
    <files>
      <file id='https://researchdata.bath.ac.uk/id/file/24096'>
        <fileid>24096</fileid>
        <datasetid>document</datasetid>
        <objectid>8749</objectid>
        <filename>fig5(a)_MMF.csv</filename>
        <mime_type>text/plain</mime_type>
        <hash>685602066e60753532979ef9fb87c896</hash>
        <hash_type>MD5</hash_type>
        <filesize>125</filesize>
        <mtime>2018-04-03 04:33:50</mtime>
        <url>https://researchdata.bath.ac.uk/441/15/fig5%28a%29_MMF.csv</url>
      </file>
    </files>
    <eprintid>441</eprintid>
    <pos>15</pos>
    <placement>15</placement>
    <mime_type>text/plain</mime_type>
    <format>other</format>
    <formatdesc>Fig5(a)_MMF.csv contains   the transmitted power through high-OH multimode fiber for one hour with pinhole in front of fiber input for optimization of coupling.</formatdesc>
    <language>en</language>
    <security>public</security>
    <license>cc_by</license>
    <main>fig5(a)_MMF.csv</main>
    <content>data</content>
  </document>
</documents>