<?xml version='1.0' encoding='utf-8'?>
<documents xmlns='http://eprints.org/ep2/data/2.0'>
  <document id='https://researchdata.bath.ac.uk/id/document/14944'>
    <docid>14944</docid>
    <rev_number>2</rev_number>
    <files>
      <file id='https://researchdata.bath.ac.uk/id/file/46867'>
        <fileid>46867</fileid>
        <datasetid>document</datasetid>
        <objectid>14944</objectid>
        <filename>Fig10_ND_Sofk_glass_with_NGP_603C.agr</filename>
        <mime_type>text/plain</mime_type>
        <hash>72f15e729f967899c3c1275b6054d75e</hash>
        <hash_type>MD5</hash_type>
        <filesize>205384</filesize>
        <mtime>2021-05-05 16:19:31</mtime>
        <url>https://researchdata.bath.ac.uk/980/46/Fig10_ND_Sofk_glass_with_NGP_603C.agr</url>
      </file>
    </files>
    <eprintid>980</eprintid>
    <pos>46</pos>
    <placement>46</placement>
    <mime_type>text/plain</mime_type>
    <format>other</format>
    <formatdesc>Figure 10 shows the total structure factors S(k) for as-prepared versus annealed glassy NAGP with x = 0, 0.4 and 0.8. The red curves give the GEM data sets and the black or blue curves give the D4c data sets, where the latter correspond to the x = 0 glass annealed at T_{TT} = 876~K for either 0.25 or 0.5~h.</formatdesc>
    <language>en</language>
    <security>public</security>
    <license>cc_by</license>
    <main>Fig10_ND_Sofk_glass_with_NGP_603C.agr</main>
    <content>data</content>
  </document>
</documents>